HUE035722 (T2)

Sulfo-aluminous clinker with a low belite content

(22) 13.03.2014

(43) 28.05.2018

(57) Summary of the corresponding patent WO2014140488 (A1): The invention relates a novel sulfoaluminous clinker with a low belite content, to a method for producing said clinker, and to the use of the clinker for producing hydraulic binder, and ultimately, grout, concrete or mortar.

(71) Vicat (FR)

Related articles:

Issue 1-2/2018 HRP20171533 (T1)

Sulfo-aluminous clinker with a low belite content

(22) 11.01.2017(43) 17.11.2017(57) Summary of the corresponding patent WO2014140488 (A1): The invention relates a novel sulfo-aluminous clinker with a low belite content, to a method for producing...

more
Issue 6/2018 PL2970009 (T3)

Novel phosphorus-doped sulfo-belitic clinker and process for its preparation

(22) 13.03.2014(43) 30.03.2018(57) Summary of the corresponding patent WO2014140487 (A1): The invention relates to a novel phosphorus-doped sulfo-belitic clinker, to a method for producing said...

more
Issue 11/2016 US 2016/0272540 A1

Method for producing a low-carbon clinker

(22) 10.03.2016 (43) 22.09.2016 (57) Method for producing a low-carbon clinker with low energy consumption comprising the following stages:...

more