Clinker substitute material made of aluminium silicate and dolomite
(22) 17.11.2015
(43) 02.06.2016
(57) The invention relates to a method for producing a clinker substitute material comprising the steps: providing a starting material containing dolomite and aluminium silicate, converting the starting material to the clinker substitute material by burning the starting material in the temperature range from > 800 to 1100 °C or by burning the starting material in the temperature range from 725 to 950 °C in the presence of a mineraliser, and cooling the clinker substitute material. The invention further relates to a binder comprising cement and to the ground clinker substitute material.
(71) HeidelbergCement AG, Berliner Strasse 6, 69120 Heidelberg (DE)
(84) ARIPO (BW, GH, GM, KE, LR, LS, MW, MZ, NA, RW, SD, SL, ST, SZ, TZ, UG, ZM, ZW), Eurasian (AM, AZ, BY, KG, KZ, RU, TJ, TM), European (AL, AT, BE, BG, CH, CY, CZ, DE, DK, EE, ES, FI, FR, GB, GR, HR, HU, IE, IS, IT, LT, LU, LV, MC, MK, MT, NL, NO, PL, PT, RO, RS, SE, SI, SK, SM, TR), OAPI (BF, BJ, CF, CG, CI, CM, GA, GN, GQ, GW, KM, ML, MR, NE, SN, TD, TG)