US 9 073 784 B2

Calcium sulfoaluminate cement with ternesite

(22) 16.07.2012

(45) 07.07.2015

(57) The present invention relates to a ternesite calcium sulfoaluminate clinker as well as a ternesite clinker containing 20 to 100 % by weight of C5S2$ and less than 15 % by weight of C4A3$, as well as the use of ternesite as an additive to calcium sulfoaluminate (ferrite) (belite) (CSA(F)(B)) clinker, calcium sulfoaluminate (ferrite) (belite) cement, and calcium sulfoaluminate (ferrite) (belite) ­binder containing 10 to 90 % by weight of CSA(F)(B) and 90 to 10 % by weight of ternesite.

(73) HeidelbergCement AG, Heidelberg (DE)

Related articles:

Issue 1-2/2018 EP 3 255 367 A1

Device for manufacturing belite calcium sulfoaluminate ternesite clinker

(22) 10.06.2016(43) 13.12.2017(57) Device for manufacturing belite calcium sulfoaluminate ternesite clinker, comprising a rotary kiln (1) and a cooler (3), wherein a tempering device (2) is provided...

more
Issue 05/2013

BCT Technology – a new alternative binder concept

The cement industry is the source of about 5 % of the global anthropogenic CO2 emissions. On average, the production of one tonne of cement clinker...

more
Issue 09/2014 HEIDELBERGCEMENT

BCT technology receives award at the CIC

From 11.–13.06.2014, the Concrete Innovation Conference (CIC) in Oslo/Norway was the meeting place for researchers focusing on future trends in the...

more